Filter by substrate, application method or viscosity – then add products to your enquiry cart.
Method
Water repellent and OGR coating for Paper/Paper boards and Kraft Papers. Total dry coat weight 7-9 GSM is recommended for best performance.
Water-based OGR Barrier CoatingsViscosity: 12-16 CPS
Air knife coater
Water repellent and OGR coating for Paper/Paper boards and Kraft Papers. A double coat with a total dry coat weight 7-9 GSM is recommended for best performance.
Water-based OGR Barrier CoatingsViscosity: 20-30 CPS
Gravure/Anilox
Water repellent and OGR coating for Paper/Paper boards and Kraft Papers. A double coat with a total dry coat weight 7-9 GSM is recommended for best performance.
Water-based OGR Barrier CoatingsViscosity: 40-60 CPS
Gravure/Anilox/Roller
Heat-sealable water-repellent and OGR barrier coating for Paper/Paper boards and Kraft Papers. Total dry coat weight 7-9 GSM is recommended for best performance.
Water-based Heat Sealable Barrier CoatingsViscosity: 12-16 CPS
Air knife coater
Note for Barrier Coatings: For higher kit values, double coat is recommended.
Heat-sealable water-repellent and OGR barrier coating for Paper/Paper boards and Kraft Papers. A double coat with a total dry coat weight 7-9 GSM is recommended for best performance.
Water-based Heat Sealable Barrier CoatingsViscosity: 25-40 CPS
Gravure/Anilox
Note for Barrier Coatings: For higher kit values, double coat is recommended.
Heat-sealable water-repellent and OGR barrier coating for Paper/Paper boards and Kraft Papers. A double coat with a total dry coat weight 7-9 GSM is recommended for best performance.
Water-based Heat Sealable Barrier CoatingsViscosity: 70-100 CPS
Gravure/Anilox/Roller
Note for Barrier Coatings: For higher kit values, double coat is recommended.
Low COF Heat seal barrier coating for flexible packaging substrates like aluminium foil, Paper, aluminium foil/Paper laminated structures for high-speed pouch making application.
Water-based Heat Sealable Barrier CoatingsViscosity: 15-35 CPS
Gravure/Anilox
Note for Barrier Coatings: For higher kit values, double coat is recommended.
Water-based heat seal coating for PVC/PET blister sealing with printed blister boards. Coating can be applied by roller coater. Note: Product not recommended for FBB boards
Water-and Solvent-based Blister CoatinggViscosity: 38-42 CPS
Water-based
Note: The ideal sealing condition are Platen Temperature: 140°C Dwell Time: 4 seconds, Pressure: 90 to 95 PSI & Coating thickness of 6 to 8 GSM.
Water-based heat seal coating for sealing of PVC blisters with printed blister boards. Coating can be applied by roller coater. Note: Product not recommended for FBB board and R-PET Blisters.
Water-and Solvent-based Blister CoatinggViscosity: 25-40 CPS
Water-based
Note: The ideal sealing condition are Platen Temperature: 140°C Dwell Time: 4 seconds, Pressure: 90 to 95 PSI & Coating thickness of 6 to 8 GSM.
Heat Seal Lacquer for sealing of PVC blisters with printed blister boards. Coating can be applied by roller coater. Note: Product not recommended for FBB board and R-PET Blisters.
Water-and Solvent-based Blister CoatinggViscosity: 45-65 CPS
Solvent based
Note: The ideal sealing condition are Platen Temperature: 140°C Dwell Time: 4 seconds, Pressure: 90 to 95 PSI & Coating thickness of 6 to 8 GSM.
Heat Seal Lacquer sealing for PVC/PET blister sealing with printed blister boards. Coating can be applied by roller coater. Note: Product not recommended for FBB boards
Water-and Solvent-based Blister CoatinggViscosity: 45-60 CPS
Solvent based
Note: The ideal sealing condition are Platen Temperature: 140°C Dwell Time: 4 seconds, Pressure: 90 to 95 PSI & Coating thickness of 6 to 8 GSM.